Defects and preventive measures of stamping and stretching parts
Time : 2023-08-30 Click count : 2700

1. Reasons for waste generation:

A. Poor quality of raw materials;

B. Improper installation, adjustment, and use of molds;

C. The worker did not feed the strip correctly along the positioning or did not ensure that the strip was fed with a certain gap;

D. Due to long-term use of the mold, there may be changes in gaps or wear on the working and guiding components of the mold;

E. Due to prolonged impact and vibration, the fastening parts of the mold become loose, causing a relative change in the installation position of the mold;

F. The operator's negligence did not follow the operating procedures.


2. The main measures to prevent waste are:

A. Raw materials must meet the specified technical conditions (strictly inspect the specifications and brands of raw materials, and conduct laboratory tests on workpieces with high requirements for dimensional accuracy and surface quality when conditions permit)

B. All aspects specified in the process specifications should be strictly followed comprehensively;

C. The tools and equipment used, such as presses and molds, should ensure that they work under normal working conditions;

D. Establish a strict inspection system during the production process, which requires a thorough inspection of the first stamped part. Only after passing the inspection can they be put into production. At the same time, inspection should be strengthened, and accidents should be dealt with in a timely manner;

E. Adhere to the civilized production system, for example, workpieces and blanks must be transported using appropriate workstation equipment, otherwise the surface of the workpiece will be crushed and scratched, affecting the surface quality of the workpiece;

F. During the stamping process, the cleanliness of the mold cavity should be ensured, and the orderly arrangement of workpieces after processing in the workplace should be neat.


3. Causes of burrs on punched parts

A. The punching gap is too large, too small, or uneven;

B. The cutting edge of the working part of the mold becomes dull;

C. Due to long-term vibration impact, the centerlines of the convex and concave molds change, and the axes do not coincide, resulting in one-sided burrs.

measures:

1) Ensure the machining accuracy and assembly quality of convex and concave molds, ensure the verticality of convex molds, withstand lateral pressure, and ensure the rigidity of the entire mold;

2) When installing the convex mold, ensure that the gap between the convex mold and the concave mold is correct, and firmly install the convex mold and the concave mold on the mold fixing plate. The end faces of the upper and lower molds should be parallel to the worktable of the press.

3) The requirements for the press include good rigidity, minimal elastic deformation, high track accuracy, and high parallelism between the pad and slider;

4) Require the pressure machine to have sufficient punching force.

The allowable height of burrs on the cut surface of punched parts

Punched sheet thickness>0.3>0.3-0.5>0.5-1.0>1.0-1.5>1.5-2.0

New trial mold burr height ≤ 0.015 ≤ 0.02 ≤ 0.03 ≤ 0.04 ≤ 0.05

The allowable burr height in production is ≤ 0.05 ≤ 0.08 ≤ 0.10 ≤ 0.13 ≤ 0.15


4. Reasons for warping and deformation of punched parts:

There are clearance forces and reaction forces on a straight line that do not generate torque. When the gap between the punch and the die is too large, the edge of the die has a conical shape, or when the contact area between the ejector and the workpiece is too small, warping deformation will occur

measures:

A. Reasonably choose the punching gap;

B. In the mold structure, a certain amount of pressure is required to increase the plane contact between the pressing plate (or support plate) and the pressing plate;

C. Check the concave die blade. If a reverse taper is found, the cutting edge of the die must be trimmed correctly.

D. When the shape of the punched part is complex and there are many inner holes, if the cutting force is uneven, the pressing force will increase. Before punching, press the strip tightly or use a high-precision press to punch it.

E. Before punching the sheet metal, it should be leveled. If the warping cannot be removed, the punched workpiece can be re leveled using a leveling mold.

F. Regularly clean the dirt inside the mold cavity, lubricate the surface of the thin sheet material, and install oil vent holes on the mold structure.


5. During punching, the accuracy of the outer edge and inner hole of the punched part decreases, and the size changes.

reason:

The position of positioning pins, blocking pins, etc. has changed or worn out excessively;

The operator's carelessness caused the material to move back and forth during feeding;

The dimensional accuracy of the strip material is low, too narrow and too wide, making it difficult to deliver to the designated location. If the strip material moves back and forth in the guide plate, the punching hole of the workpiece will have a significant deviation from the front and rear positions of the outer shape.


6. Reasons for non-conforming bending dimensions and shapes of parts

A. The rebound of the material causes the product to be unqualified

Measures to reduce rebound:

Choose stamping materials with stable mechanical properties, high elastic modulus, and low yield point;

Add calibration program and use calibration bending instead of free bending;

Before bending, the material should be annealed to soften the cold work hardened material before bending into shape;

If there is shape deformation during stamping, it is difficult to remove; Then change or adjust the slope of the convex and concave molds, and the gap between the convex and concave molds should be equal to the minimum material thickness.

Increase the contact area between the concave mold and the workpiece, and reduce the contact area between the convex mold and the workpiece.

Reduce the impact of rebound by overcorrecting.

B. If the locator is worn and deformed, causing inaccurate positioning of the strip, a new locator must be replaced.

C. In non guided bending molds, improper adjustment of the bottom dead center position of the press slide during adjustment on the press can also result in the shape and size of the bent part being non-conforming.

D. If the pressing device of the mold malfunctions or does not work at all, it is necessary to readjust the pressing force or replace the pressure spring to make it work normally.


7. Cracks appear at the bending part of the bent part (the internal stress in the bending deformation zone exceeds the material strength limit)

A. Removing burrs outside the curved area can lead to stress concentration in that area,

1) Reduce bending deformation

2) Remove burrs from the area

3) Place the side with burrs inside the curved area

B. When bending workpieces, it is best to make the bending direction perpendicular to the fiber direction (rolling direction) of the material.

C. The bending radius should not be too small, and if the quality allows, the fillet radius should be increased as much as possible.

D. The surface of the bent blank should be smooth, without obvious protrusions or scars.

E. Intermediate annealing process is used to remove internal stress during bending, and softening bending rarely produces cracks.

F. When bending, larger bending parts must be coated with lubricant to reduce friction during bending.


8. Deviation of bent parts during bending process

During the bending process, when the blank slides along the surface of the concave mold, it will experience frictional resistance. If the frictional resistance on both sides of the blank is significantly different, the blank will move towards the side with greater frictional resistance.

measures:

1) Asymmetric bending parts are formed by symmetrical bending (single-sided bending parts are cut after two symmetrical bends)

2) Add an elastic compression device on the bending mold to compress the billet and prevent it from moving during bending.

3) Utilize internal holes and external positioning forms to ensure accurate positioning.


9. Reasons and solutions for surface scratches on curved parts.

A. When continuously bending soft materials such as copper and aluminum alloys, metal particles or slag are prone to adhere to the surface of the working area, causing significant scratches on the parts. At this time, it is necessary to carefully analyze and study the shape and lubricating oil of the working parts, and it is best to avoid particles and slag on the blank, which can cause scratches.

B. When the bending direction is parallel to the rolling direction of the material, cracks will appear on the surface of the workpiece, reducing the surface quality of the workpiece. When two or more parts are bent, ensure that the bending direction is as close as possible to the rolling direction.

C. When the burr surface is bent as the outer surface, the parts are prone to cracking and scratching; Therefore, the burr surface should be considered as a curved inner surface.

D. The fillet radius of the concave mold is too small, and there are impact marks on the curved part. Polishing the concave mold and increasing the fillet radius of the concave mold can avoid wear on bent parts.

E. The gap between the convex and concave molds should not be too small, otherwise it will cause thinning and wear. Regularly check the changes in mold clearance during stamping.

F. If the depth of the convex mold entering the concave mold is too large, there may be scratches on the surface of the part. Therefore, while ensuring that it is not affected by rebound, the depth of the convex mold entering the concave mold should be appropriately reduced.

G. In order to meet the precision requirements of the parts, bottom pressing bending molds are often used. When bending, the springs, locating pin holes, support plates, and return holes on the pressing plate will be pressed into indentations and should be adjusted.


10. What is the reason for the change in the position of the blank hole during bending? How to exclude

A. The position and size of the hole are incorrect, resulting in thinning due to bending and stretching

Measures: Strictly control the bending radius, bending angle, and material thickness; Trim the neutral layer of the material so that the depth of the convex mold entering the concave mold and the depth of the convex and concave molds are appropriately consistent.

B. Reasons for non concentric holes

1) Insufficient bending height. 2) The blank slides. 3) Rebound. 4) The curved plane exhibits undulations.

measures:

1) Ensure the correct left and right bending height.

2) Correct the worn positioning pins and plates.

3) Reduce rebound and ensure the parallelism and flatness of the two curved surfaces.

4) Change the process route, first bend and correct before punching.

C. The bending curve is not parallel to the centerline of the two holes, and the part with a bending height less than the minimum bending height shows an outward opening shape after bending.

measures:

1) When bending, the minimum bending height H (H ≥ R 2t t material thickness R bending radius) should be ensured.

2) Change the shape of the processed parts and remove parts with a bending height less than the minimum without affecting their use.

D. Holes near curved lines are prone to deformation.

measures:

1) When designing bent parts, ensure that the edge distance X from the bent part to the hole is greater than a certain value X ≥ (1.5-2.0) t t t of the bent sheet thickness.

2) Designing auxiliary holes in the bending area to absorb bending deformation stress can prevent hole deformation near the bending curve. Generally, the scheme of bending first and punching later is adopted.


11. After bending, the bent parts show significant thinning

A. The bending radius is too small relative to the plate thickness value (r/t>3 right angle bending). Generally, increasing the bending radius is used.

B. Multi angle bending makes the bent part thinner and larger. In order to reduce thinning, the single angle multi process bending method should be used as much as possible.

C. When using a pointed convex mold, the convex mold enters the concave mold too deeply, significantly reducing the thickness of the bent part.


12. Reasons and prevention of flange wrinkling during deep drawing process of deep drawn parts

reason:The edge pressure on the flange is too small to resist excessive tangential compressive stress; And it causes tangential deformation, resulting in the formation of folds after losing stability. Thinner materials are also prone to wrinkle formation.

measures:Increase the edge pressure of the edging ring and appropriately increase the thickness of the material.


13. Reasons and prevention of wall cracking in deep drawn parts

reason:

A. Excessive radial tensile stress of the material during stretching;

B. The radius of the concave mold fillet is too small,

C. Poor lubrication during deep drawing;

D. The plasticity of raw materials is poor.

measures:

1) Reduce the edge pressure.

2) Increase the fillet radius of the concave mold.

3) Proper use of lubricants.

4) Choose materials with better performance or add annealing processes in the workshop.


14. The bottom of the deep drawn part is cracked by pulling

The reason is that the fillet radius of the concave mold is too small, which causes the material to be cut. (Usually occurring in the early stage of deep drawing) Increasing the fillet radius of the concave die reduces the surface roughness of its smooth transition, usually Ra<0.2 μ m.


15. The edges of the deep drawn parts are uneven and wrinkled.

reason:The blank and the center of the convex concave die are not in a straight line or the material thickness is uneven. The radius of the concave die corner is uneven with the gap between the convex concave die (if the radius of the concave die corner is too large, the edge pressing ring and the edge pressing ring will separate in the final stage of deep drawing, and the material that does not cross the corner cannot be pressed into the edge pressing ring and wrinkled before being pulled into the concave die to form mouth edge wrinkles).

measures:Repositioning the die, before putting it into production, adjust the fillet radius of the concave die and the clearance between the convex and concave dies to make them uniform in size (reducing the fillet radius of the concave die or using an arc-shaped edge pressing ring device can remove wrinkles)


16. Reasons and preventive measures for wrinkling at the waist during deep drawing of conical or hemispherical parts:

reason:At the beginning of deep drawing, most of the material is in a suspended state, with too little edge pressure, too large fillet radius of the die, or excessive use of lubricant. The radial tensile stress decreases, and the material loses stability under tangential compressive stress, resulting in wrinkles.

measures:Increase the edge pressure or adopt a rolled rib structure, reduce the fillet radius of the concave die or slightly increase the material thickness.


17. Reasons and preventive measures for drawing marks on the surface of deep drawn parts

reason:

A. If there are sharp scratches on the surface of the convex or concave mold, resulting in corresponding tensile marks on the surface of the workpiece, the surface should be polished or buffed.

B. The gap between the convex and concave molds is too small or uneven, causing scratches on the surface of the workpiece during deep drawing. At this time, the gap between the convex and concave molds should be adjusted until it is suitable.

C. The concave die has a rough rounded surface, and the workpiece surface is scratched during stretching. At this point, the radius of the rounded corners of the concave mold should be polished and smoothed.

D. During stamping, impurities are mixed into the working surface or material surface of the die due to uncleanliness, which damages the surface of the workpiece. Therefore, the surface of the convex and concave molds must always be kept clean during material pulling, and the blank must be wiped before pulling;

E. When the hardness of the convex and concave molds is low, metal shavings will adhere to their surfaces, and there will also be stretch marks on the surface of the deep drawn workpiece. Therefore, in addition to increasing the hardness of the convex concave die surface, even if the remaining metal waste is removed, the surface of the convex concave die should always be inspected.

F. Poor quality lubricants can also increase the surface roughness of deep drawn workpieces. In this case, lubricants suitable for deep drawing processes should be used, and if necessary, the lubricant should be filtered before use. Thus preventing impurities from entering and damaging the surface of the workpiece.


18. What is the reason for the unevenness of the straight wall of the deep drawn part?

reason:

A. There are no ventilation holes designed and manufactured on the convex mold, so the surface of the convex mold will deform due to compressed air, resulting in unevenness. In this case, ventilation holes must be added.

B. The rebound of the material can also cause unevenness on the surface of the deep drawn workpiece, and finally, a shaping process needs to be added.

C. The gap between the convex and concave molds is too large, making it difficult to flatten during deep drawing. At this time, the gap must be uniformly adjusted.

News Related news
凹凸国产熟女精品视频APP| 精品国产亚洲AV麻豆| 少妇BBWBBW高潮| 国产成人精品日本亚洲专区不卡 | 欧美精产国品一二三区别| 锕锕锕锕锕锕锕锕轻点好疼视频 | 70歳の熟女セックス| 人妻系列无码专区免费视频 | GAY亚洲男男GV在线观看网站| 日本XXX色视频在线观看| 国产成人综合久久久久久| 亚洲大尺度专区无码| 裸体美女洗澡啪啪裸J网站| 暗交小拗女一区二区三区电影| 婷婷成人小说综合专区| 精品亚洲国产成人小电影| 97碰碰碰人妻无码视频| 四虎影视永久无码精品| 精品久久久无码人妻字幂| 98色精品视频在线| 特级毛片A级毛片在线播放WWW| 精品国产一区二区三区不卡在线| 97精品伊人久久久大香线蕉| 日韩夜夜高潮夜夜爽无码| 国产亚洲欧美日韩俺去了| 荫蒂每天被男人添| 日韩精品无码人妻一区二区三区| 国模少妇一区二区三区咪咕| 中国女人内射6XXXXXWWW| 日韩精品无码一区二区三区AV| 国产在线精品无码二区| 中文乱码字幕高清一区二区| 色综合天天综合网天天小说| 精品人妻暴躁一区二区三区| PYTHON人马大战CSDN| 五月丁香色综合久久4438| 老司机久久99久久精品播放| 纯肉高H爽文粗大| 亚洲国产精品久久久天堂麻豆宅男| 女人下边水润紧致好处| 国产精品电影久久久久电影网| 夜里18款禁用软件APP| 日本熟妇色XXXXXBBB日本| 狠狠色噜噜狠狠狠888米奇| 9久9久女女免费视频精品| 无码精品国产一区二区三区免费 | 中国在线观看免费高清完整版| 日韩国产欧美亚洲V片| 狠狠色综合久久丁香婷婷| AVTT天堂网久久精品| 小嫩妇里面又嫩又紧| 乱色熟女综合一区二区三区| 丰满少妇被猛烈进入无码| 亚洲色偷偷综合亚洲AV伊人| 日本在线视频WWW鲁啊鲁| 精品国产污污免费网站| 把腿张开老子臊烂你多p晓晓| 亚洲AV永久无码精品尤物在线| 欧美黑人一区二区| 国产又粗老女人又硬又爽| 99久久久国产精品消防器材| 性色AV无码久久一区二区三区| 女人被男人吃奶到高潮 | 2012电影在线观看神马影院| 无码人妻精品一区二区蜜桃网站| 麻豆MDX0020穷小子大翻身| 国产极品熟女沙发内射AV| 在线观看亚洲区激情AV| 天天躁夜夜躁AV天天爽| 麻豆视传媒官方直接进入| 国产后入又长又硬| 51成品网站W灬源码1688| 亚洲性色AV私人影院无码| 日本老熟妇wwwbbb| 久久A级毛片免费观看| 成人片黄网站色大片免费观看AP| 亚洲色欲色欲综合网站色偷偷| 日日摸夜夜添夜夜添AV| 久久婷婷五月综合成人D啪 | 精品无码国产污污污免费网站国产| 锕锕锕锕锕锕锕轻点好痛免费| 亚洲精品卡一卡2卡3卡4卡| 日韩精品成熟妇人Av一区二区 | 荡公乱妇第1章95| 野花在线高清视频| 我和亲妺妺乱的性视频| 欧美成在线精品视频| 火柴人战争遗产破解版| 处破痛哭A√18成年片免| 伊人久久大香线蕉AV仙人| 无码一区二区波多野结衣播放搜索| 女人18片毛片60分钟630| 激情内射亚洲一区二区三区爱妻 | 不卡AV电影在线| 亚洲一线产区二线产区区别在哪里 | 日日噜噜夜夜狠狠视频| 久久久久亚洲AV成人无码| 亚洲高清成人AV电影网站| 色视频综合无码一区二区三区| 欧美大屁股妞性潮喷ⅩXX| 久久99亚洲含羞草影院| 国产精品成人3p一区二区三区| JAPANESEHD日本乱厨房| 亚洲日韩一页精品发布| 日产精品1卡二卡三卡| 男人边做边吃奶头视频| 玩弄丰满熟妇乱XXXXX性多毛| 久久精品国产一区二区三| 国产成人无码AV一区二区在线观| 性欧美牲交在线视频| 亚洲AV无码专区在线电影成人| 日本成熟…@视频| 老师趴讲台屁股撅起来作文| 国产尤物AV尤物在线观看| 成熟丰满熟妇高潮XXXXX| √天堂资源BT在线官网| 亚洲AV无码专区亚洲AV紧身裤 | 亚洲熟妇无码久久精品导航| 无码福利日韩神码福利片| 人妻人妇人妻一区二区三区| 久久人人97超碰精品| 国产午夜福利精品久久2021| 成熟丰满熟妇AV无码区| 2023国产精品一卡2卡三卡| 亚洲浮力影院久久久久久| 特黄特色三级在线观看| 热RE99久久精品国99热| 两根硕大一起挤进小紧H共妻| 果冻十麻豆十天美十老师| 国产AV剧情MD精品麻豆| でも私はあなたより賢いです意思| 又黄又爽又色的视频| 亚洲高清国产拍精品熟女| 玩爽少妇人妻系列无码| 日本老熟妇毛茸茸| 免费人成在线观看视频高潮| 久久精品无码一区二区WWW| 国内精品久久久久久中文字幕| 国产AⅤ精品一区三区| japanese国产在线观看| 中国少妇精品久久久久无码AV| 亚洲精品亚洲人成人网| 亚洲A∨精品无码一区二区| 视频视频APP在线看| 人妻夜夜爽天天爽三区| 女人来高潮水多视频| 乱码AV麻豆丝袜熟女系列| 九九九九精品视频在线观看| 国产亚洲日韩一区二区三区| 国产精品99久久99久久久动漫| 成人无码H动漫在线网站樱花| CAOPORN最新地址| 中文字幕人妻AV一区二区| 一本一道AⅤ无码中文字幕| 天码AV高清毛片在线看_| 日韩AⅤ人妻无码一区二区| 欧洲女人牲交视频免费| 女人被弄到高潮的免费视频APP| 老妇饥渴XXHDⅩXXOOO| 久久99国产精品久久| 韩国亚洲精品a在线无码| 国产私人尤物无码不卡| 国产精品免费_区二区三区观看 | CAOPOREN超碰最新地址| 中文字幕AV无码一区二区蜜芽三| 亚洲一区二区三区日本久久九| 亚洲国产成人精品激情姿源| 亚洲 无码 国产精品| 午夜天堂一区人妻| 无码精品国产VA在线观看DVD| 四季亚洲精品成人AV无码网站 | 亚洲精品国产精品乱码不卡√| 亚洲AVTV永久综合在线| 无码精品人妻一区二区| 天天躁日日躁很很躁2022| 深田えいみ禁欲后被隔壁人妻| 日韩一区二区三区无码影院| 日本免费一区二区三区最新VR| 人人妻人人澡人人爽人人精品97| 欧美性极品少妇精品网站| 欧美电影在线观看| 女人被弄到高潮叫床免| 欧美成人猛片AAAAAAA| 你下水好多下水道BD| 免费专区SM美脚践踏调教视频| 免费看无码自慰一区二区| 蜜臀成人片免费视频在线观看| 免费萌白酱国产一区二区三区 | 少妇人妻激情乱人伦| 色五月丁香五月综合五月4438| 日韩精品一区二区三区在线观看 | 中文字幕免费不卡二区| 曰本女人牲交视频视频免费| 玉米地诱子偷伦初尝云雨孽欲| 一线产区与二线产区的定义| 一本色道久久综合一| 中文乱码35页在线观看| 中文字幕亚洲一区二区VA在线| 7777888888精准管家婆| CHRISTMAS农村夫妻HO|